濟南抹面砂漿:回填溝槽的裂縫
來源:http://www.laodaohe.cc 日期:2025-08-30 發布人:
所謂的溝槽邊緣的裂縫,主要就是針對家里在水電改造的時候,墻面上所開的溝槽接縫。在溝槽內布置水管線管之后,一般都是使用相應的材料對溝槽進行恢復,在恢復過程中沒有處理好就可能出現裂縫。常見原因如下:
The so-called cracks at the edge of the groove are mainly aimed at the joints of the grooves opened on the wall during the water and electricity renovation at home. After arranging water pipes in the trench, corresponding materials are usually used to restore the trench. If not properly treated during the restoration process, cracks may occur. The common reasons are as follows:
原因分析
Cause analysis
?、倩靥顪喜鄣臅r候,溝槽內回填材料不密實。使用回填材料來回填溝槽的時候沒有將內部填塞密實,例如管道底部虛空的,就容易造成溝槽的開裂。
?、?When backfilling the trench, the backfill material inside the trench is not dense enough. When using backfill materials to fill the trench back and forth, if the interior is not filled tightly, such as the void at the bottom of the pipeline, it is easy to cause the trench to crack.
②溝槽回填材料選擇不正確。對于水電的溝槽,個人認為應該是高強的水泥砂漿或者是細石混凝土回填,不允許使用粉刷石膏回填。
?、?The selection of backfill material for the trench is incorrect. For water and electricity trenches, I personally believe that high-strength cement mortar or fine aggregate concrete should be used for backfilling, and the use of plaster for backfilling is not allowed.
③回填以后,沒有對溝槽的回填材料進行養護。例如使用水泥砂漿回填溝槽,沒有及時的灑水養護,導致水泥砂漿失水而出現了開裂。
?、?After backfilling, the backfill material for the trench was not cured. For example, using cement mortar to backfill trenches without timely watering and curing resulted in cement mortar losing water and cracking.
處理方法
Handling method
?、偈紫葘喜坶_裂部位的混凝土或者是水泥砂漿輕輕的剔鑿掉,這時一定要注意不要破壞里面的管線。
?、?Firstly, gently chisel off the concrete or cement mortar at the cracked part of the trench, and be sure not to damage the pipelines inside.
②在溝槽的內部使用掛鋼絲,鋼絲網一定要掛嚴實。
?、?Use hanging steel wire inside the groove, and the steel wire mesh must be hung tightly.
?、劢ㄗh大家使用水泥砂漿抹,涂抹的時候最起碼要分兩遍來進行。如果通過水泥砂漿的厚度超過了30mm,需掛兩層鋼絲網。抹灰第一遍完成以后在表面再掛一次,以此增強其抗裂的能力。
③ It is recommended that everyone use cement mortar to apply, and at least two coats should be applied. If the thickness of the cement mortar exceeds 30mm, two layers of steel wire mesh need to be hung. After the first coat of plastering is completed, hang it again on the surface to enhance its crack resistance.
本文由 濟南抹面砂漿 友情奉獻.更多有關的知識請點擊 http://www.laodaohe.cc/ 真誠的態度.為您提供為全面的服務.更多有關的知識我們將會陸續向大家奉獻.敬請期待.
This article is a friendly contribution from Jinan plaster mortar For more related knowledge, please click http://www.laodaohe.cc/ Sincere attitude To provide you with comprehensive services We will gradually contribute more relevant knowledge to everyone Coming soon.